Testing & certification
A marking is a legal claim. We test before we make one.
01 / THE TESTS
Four procedures
What we actually do in the cell
Visual & dimensional
Design type confirmed, wall thickness checked, marking legibility assessed.
Leak test
Internal air pressure held and monitored. Every unit, every time.
Hydrostatic test
Where the design type and intended cargo require it. Pressure and hold time logged.
Re-mark
New marking pressed with our reconditioner code and the month and year.
Drop testing is a design-qualification test, not a periodic one, and we do not perform it. If you need design qualification for a new container type, that is a job for an accredited test laboratory and we will point you at one.
02 / READING THE MARK
What UN 31HA1/Y actually tells you
Each character is a fact. 31 is a composite IBC for liquids. HA1 is a plastic inner receptacle in a steel outer frame. Y is packing group II and III service. After that comes the month and year of manufacture or reconditioning, the country code, the manufacturer or reconditioner code, the stacking load, and the maximum permitted gross mass.
A marking without a legible date is not a valid marking. A marking on a unit that has been cut, ported or otherwise modified is not a valid marking either — which is why our fabrication bay grinds marks off before the plasma torch comes out.
The full character-by-character breakdown lives on the UN marking decoder.
Service details
- Leak test, per unitIncluded in reconditioning
- Hydrostatic testOn request or where required
- Re-markingAfter pass, same visit
- Your containersAccepted, toll basis
- DocumentationTest result sheet per unit
- Records retained7 years
- Failure handlingRebottle quote or scrap credit
- Turnaround2–4 business days
One thing we will not do
We will not re-mark a container whose prior cargo we cannot document, even if it passes every test. A marking says the container is fit for regulated service; without a cargo history we cannot make that claim honestly.
How long is a UN marking valid?
For a composite IBC in regulated liquid service, periodic retesting is required at intervals set by the regulation — generally a leak test every two and a half years and a full inspection every five. The marking date tells you where you are in that cycle. We will test and re-mark on schedule if you put your fleet on a standing booking.
Can you certify a tote I bought somewhere else?
We can test it and, if the design type is intact and the cargo history is documented, re-mark it. If either of those is missing, we can test it and issue a result — but not a marking.
What is the failure rate?
Around 6% of units entering the cell fail leak test, almost always at the valve flange or the lid gasket rather than the bottle wall. Most of those are fixed with a $14 gasket and re-tested the same day.
A / SPECIFICATION
Reference
Dimensions, fittings and seat materials
Fig. 1
Fig. 2| Capacity | Litres | Footprint | Height | Tare | Gross (water) | Stack loaded |
|---|---|---|---|---|---|---|
| 275 gal | 1,041 | 48 × 40 in | 46 in | ≈140 lb | ≈2,435 lb | 2 high |
| 330 gal | 1,249 | 48 × 40 in | 53 in | ≈155 lb | ≈2,905 lb | 2 high |
| 350 gal | 1,325 | 48 × 40 in | 56 in | ≈165 lb | ≈3,075 lb | 2 high |
| 120 gal | 454 | 40 × 32 in | 38 in | ≈95 lb | ≈1,095 lb | 2 high |
| 180 gal | 681 | 42 × 36 in | 42 in | ≈115 lb | ≈1,616 lb | 2 high |
| 550 gal | 2,082 | 60 × 48 in | 60 in | ≈240 lb | ≈4,830 lb | 1 high |
B / FITTINGS
What threads onto it
Fittings, threads and seat materials
| Fitting | Size | Seals by | Seat options | Typical service |
|---|---|---|---|---|
| S60x6 butterfly valve | 2 in | Flat gasket face | EPDM, Viton, PTFE | The standard IBC outlet |
| S70x6 butterfly valve | 2 in | Flat gasket face | EPDM, Viton | European and some 330 gal units |
| 2 in NPT ball valve, poly | 2 in | Thread flanks + tape | EPDM, Viton | Retrofits, metered dispensing |
| 2 in NPT ball valve, stainless | 2 in | Thread flanks + tape | PTFE | Solvents, pressure, hot cargo |
| 3 in butterfly valve | 3 in | Flat gasket face | EPDM, Viton | Viscous cargo, high flow |
| 6 in fill cap | 6 in | Gasketed lid | EPDM, silicone | Vented or solid — choose deliberately |
| Camlock adapter, type C | 1.5 / 2 in | Cam arms + gasket | Buna, Viton | Repeated connect / disconnect |
| Bulkhead tap | 3/4 in | Both-side gaskets | Brass, poly | Rain kits, site water |
| Material | Good with | Avoid with | Temperature | Cost |
|---|---|---|---|---|
| EPDM | Water, acids, caustics, brine, ag-chem | Oils, fuels, aromatics | -40 to 250 °F | Low |
| Viton (FKM) | Solvents, oils, fuels, aromatics | Ketones, amines, hot steam | -15 to 400 °F | High |
| Nitrile (NBR) | Oils, diesel, greases, hydraulics | Ozone, strong oxidisers | -30 to 250 °F | Low |
| PTFE envelope | Almost all chemistry, high purity | Needs very flat flange faces | -100 to 450 °F | High |
| Silicone | Food contact, wide temperature | Solvents, abrasion | -60 to 450 °F | Medium |
E / GRADING
A grade is a promise, not a mood
How every unit is scored
| # | Point | Critical? |
|---|---|---|
| 01 | Prior cargo declaration — present, written, specific | Yes |
| 02 | Residual liquid — any volume at all | Yes |
| 03 | Odour after wash — fixed odour by trained nose | Yes |
| 04 | Bottle corner stress whitening | No |
| 05 | Interior scoring you can feel | No |
| 06 | Interior crazing — fine surface cracking | Yes |
| 07 | Bottle bulge or deformation | Yes |
| 08 | Wall thickness at the thinnest point | Yes |
| 09 | Dome port condition and flange flatness | No |
| 10 | Outlet threads — cross-threading, chipping | Yes if crossed |
| 11 | Valve function, full open and close | No, replaceable |
| 12 | Gasket condition — compression set, bloom | No, replaceable |
| 13 | Cage squareness along the top rail | No, pressable |
| 14 | Cage weld integrity at tube intersections | Yes |
| 15 | Cage coating and galvanising loss | No |
| 16 | Pallet condition — cracked feet, rot, corrosion | No, replaceable |
| 17 | Forklift pocket integrity | No |
| 18 | UN marking legibility and date | No, re-markable |
| 19 | Leak test under our procedure | Yes |
D / ORDERING
Commercial terms, up front
Lead times, minimums and what happens when it goes wrong
| Item | Detail |
|---|---|
| Minimum order | One unit. No account minimum, no membership. |
| Stock lead time | Grade A and B 275 gal usually ship the same week |
| Rebottled lead time | 2–3 weeks, built to order in bay D |
| Food-grade lead time | 1–3 weeks when stock exists; supply-dependent |
| Full truckload | 45 on a 48 ft flat, 48 in a 53 ft van, 90 empties double-stacked |
| Payment, first order | Prepay by ACH or card |
| Payment, established | Net 30 on credit approval |
| Grade guarantee | Regrade or replace, our freight both ways, 14 days |
| Leak warranty | 30 days from delivery, normal atmospheric service |
| Cancellation | Free until the truck is loaded |
| Returns | 14 days on unused stock units, freight at your cost |
| Sales tax | Indiana resale certificates and out-of-state equivalents accepted |
G / PITFALLS
Learned the expensive way
Five mistakes that cost people money
Ordering a 330 without measuring the ceiling
A 275 and a 330 share a footprint; the 330 is seven inches taller. Two 330s stacked is 110 inches against 96 for two 275s, and most sprinkler regimes want eighteen inches of clearance below the deflector. That seven inches is frequently the whole margin.
Forcing an NPT fitting into an S60x6 port
Both are roughly two inches, so it bites and feels tight. It is not sealing, it is chewing the buttress thread. The joint weeps two days later, usually in transit, and cross-threading is one of the few faults that condemns an otherwise perfect bottle.
Reusing a flange gasket
A gasket is a one-use part the moment it has taken a compression set. Reusing one is the cause of most 'the new valve still leaks' emails we get. They cost a couple of dollars. Keep a box at the fill point.
Specifying a solid lid on a tote that sees sun
Sealed container, rising temperature, nowhere for the expansion to go. The bottle bulges between the cage bars and does not fully return. A vented lid is the cheapest risk control in this industry.
Ignoring specific gravity
A full 275 of water is 2,435 lb. The same tote of UAN 32 is 3,168 lb, and a 330 is 3,785 lb. Plenty of lift-gates are rated at 2,500 or 3,000 lb, and the rating assumes a centred load.
F / END OF LIFE
Reuse first, recycle last
What happens when the container is finally finished
| Step | Outcome | Share of mass | Cost to us |
|---|---|---|---|
| 01 | Reuse as is — wash and redeploy | 63.9% | 11 gal of mostly reclaimed water |
| 02 | Repair and reuse — valve, gasket, pallet, cage | 11.4% | Parts and bench time |
| 03 | Rebottle — new bottle, reclaimed steel | 9.6% | A new bottle, two thirds of mass retained |
| 04 | Upcycle — rain kits, grow beds, wash stations | 3.2% | Fabrication time |
| 05 | Material recovery — HDPE regrind, steel, wood | 11.3% | Grinding, washing, drying energy |
| 06 | Residual to licensed disposal | 0.6% | Sludge, gasket rubber, fasteners, laminates |



Toll testing available